Penofin Hardwood Application

For optimum performance bring the stain to room temperature before application.
Penofin hardwood application. For some hardwood applications pre sand the surface with 60 to 80 grit sandpaper. Penofin for hardwood is especially formulated to penetrate dense hardwoods and. How to apply penofin penetrating oil finish for hardwood to a hardwood deck. Hardwood when it comes to hardwood most architects contractors and consumers trust penofin for hardwood to bring out the natural beauty of the wood.
Apply penofin to a clean dry surface. Penofin exterior wood finishes wood stains and wood care products set the bar for quality durability and ease of maintenance among discerning consumers craftsmen and professionals. Simply wash the surface with water and a mild detergent. 2 coat application is recommended.
Minimum temperature is 45 degrees fahrenheit. Because penofin is a low solid product there is no stripping or sanding necessary. Stir can thoroughly before use. Penofin is stable under freeze thaw conditions.
Do not apply if the wood is hot to the touch. The results are always outstanding. Apply at temperatures above 45. Surface must be free of dirt and sawdust build up.
One gallon of penofin exotic hardwood stain provides 300 400 square feet of coverage. Easy to apply and maintain penofin for hardwood enhances the grain and natural ric. See how penofin for hardwood brings this southern california deck to life. Follow the application methods listed on the previous page for a fresh and beautiful wood surface.
Penofin allows wood to breathe important in working with exotic hardwoods such as mahogany teak ipe brazillian redwood and many other species. Apply a light coat to clean dry unfinished wood by using a stain pad pump sprayer or high quality china bristle brush. For best results a pad applicator is recommended over large deck areas or a high quality natural bristle brush. Only penofin penetrating oil finish can meet the needs of hardwood in fiber protection penetration stabilizing and nourishing.
Do not over apply or surface will become tacky or sticky. Made in america independent proud.